| Material Designation | AlMgSio.5F25 |
|---|---|
| Material Number | Al6063-T5 |
| Minimum Tensile Strength | 250N/mm2 |
| 0.2% Proof Stress | 160N/mm2 |
| Ductile Yield A5 | 10% |
| Ductile Yield A10 | 8% |
| Modulus of Elasticity | 70 000N/mm2 |
| Brinell Hardness | 75HB |
| Coefficient of Thermal Expansion | (-50_+20°C) =21.8x10-51/K (+20_+100°C) =23.8x10-61/K |
| Transversal Contraction Figure | V = 0.34 |
| Anodizing Process | E6/EV1 Clear |
| Thickness of Layer | 10µm |
| Hardness | 300HV |
| Section Faces Are Parallel Within 0.1mm | +/-0.1mm |
| Straightness of Profile - Maximum Deviation of 0.3mm per 300mm | 300mm 0.3mm |
| Maximum twist is 1.5mm per 2000mm | 2000mm 1.5mm |